| COMPOSITION | % |
| Carbon | 0.01 |
| Manganese | 1.7 |
| Silicon | 0.8 |
| Phosphorous | 0.015 |
| Sulphur | 0.01 |
| Chromium | 18.5 |
| Nickel | 12.8 |
| Molybdenum | 2.6 |
| Copper | 0.15 |
| Ferrite number | 6 |
| MECHANICAL | AS WELDED |
| Tensile strength | 570 MPa |
| 0.2% Proof stress | 435 MPa |
| Elongation on 4d | 42% |
| Elongation on 5d | 40 % |
| Impact energy @ -130°C | < 70 J |
| Impact energy @ -196°C | 30 – 60 J |